MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chemours Krytox™ AGL 829 PFPE Performance Lubricant
Categories: Fluid; Lubricant; Perfluoropolyether (PFPE)

Material Notes: Krytox™ AGL 829 grease contains extreme pressure and anti-corrosion additives grease for aviation gearbox applications. Typical applications include those in potentially corrosive atmospheres, where vibrational or shock loading may be significant and an element will spend more time experiencing mixed film or boundary lubrication versus the desired full film or hydrodynamic lubrication. Krytox™ AGL 829 grease is specifically designed to lubricate gears and their associated bearings under relatively low temperature conditions

Information provided by Chemours Krytox

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.10 g/cc
@Temperature 0.000 °C
2.10 g/cc
@Temperature 32.0 °F
Volatiles  2.0 %
@Treatment Temp. 121 °C,
Time 79200 sec
2.0 %
@Treatment Temp. 250 °F,
Time 22.0 hour
D972
 5.0 %
@Treatment Temp. 204 °C,
Time 79200 sec
5.0 %
@Treatment Temp. 399 °F,
Time 22.0 hour
D972
Viscosity Measure  40 cSt
@Temperature 40.0 °C
40 cSt
@Temperature 104 °F
base oil
 100 cSt
@Temperature 100 °C
100 cSt
@Temperature 212 °F
base oil
 590 cSt
@Temperature 0.000 °C
590 cSt
@Temperature 32.0 °F
base oil
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 120 °C248 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
 
Descriptive Properties
AppearanceYellow, Creamy Consistency
Standard NLGI Grade0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WDUPJ823 / 254011

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.