MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Copper Alloy, UNS C64760, H02 Temper, Flat Products
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: 1/2 Hard

Fabrication Properties: Excellent Suitability – Soldering, Capacity for Being Cold Worked, Capacity for Being Hot Formed; Good Suitability – Brazing, Gas Shielded Arc Welding, Coated Metal Arc Welding, Spot Weld

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.89 g/cc0.321 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 178
@Load 0.500 kg
178
@Load 1.10 lb
Tensile Strength 572 MPa83000 psi
Tensile Strength, Yield 517 MPa75000 psi0.2% Offset
Elongation at Break 10 %10 %
Tensile Modulus 87.6 GPa12700 ksi
Modulus of Rigidity 33.1 GPa4800 ksi
Poissons Ratio 0.320.32Calculated
Machinability 20 %20 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000370 ohm-cm0.00000370 ohm-cm47% IACS
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
Thermal Conductivity 16.41 W/m-K113.9 BTU-in/hr-ft²-°F
Melting Point 1068 - 1087 °C1954 - 1989 °F
Solidus 1068 °C1954 °F
Liquidus 1087 °C1989 °F
Annealing Point >= 450 °C>= 842 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature >= 250 °C>= 482 °FStress Relief
Hot-Working Temperature 800.0 - 950.0 °C1472 - 1742 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu >= 93.5 %>= 93.5 %
Lead, Pb <= 0.020 %<= 0.020 %
Magnesium, Mg <= 0.050 %<= 0.050 %
Nickel, Ni 0.40 - 2.5 %0.40 - 2.5 %
Silicon, Si 0.050 - 0.60 %0.050 - 0.60 %
Tin, Sn <= 0.30 %<= 0.30 %
Zinc, Zn 0.20 - 2.5 %0.20 - 2.5 %
 
Descriptive Properties
Proportional Limit58 ksi
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC64760x1 / 292239

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.