MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger TECATEC PEEK CF50 S280 CP/IP/OS V01 natural Polyetheretherketone, 50% Carbon Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes:
  • excellent chemical resistance
  • low coefficient of thermal expansion
  • continuous service temperature up to 260 °C
  • very high stiffness
  • very high strength
Target Industries:
  • automotive industry
  • mechanical engineering
  • oil and gas industry
  • safety engineering
  • sporting goods

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.52 g/cc
Filler Content 50 %Fiber volume
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 713 MPaISO 527-4
Modulus of Elasticity 59.0 GPaISO 527-4
Flexural Strength 866 MPaISO 14125
Flexural Modulus 55000 MPaISO 14125
Compressive Strength 645 MPaISO 14126
Shear Strength 65.0 MPaInterlaminar; ISO 14130
 137 MPaInterplanar; ISO 14129
Charpy Impact Unnotched 65.5 kJ/m²
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 5.00 µm/m-°C
CTE, linear, Transverse to Flow 5.00 µm/m-°C
Melting Point 343 °C
Maximum Service Temperature, Air 260 °Clong term
 300 °Cshort term
Glass Transition Temp, Tg 143 °C
 
Processing PropertiesOriginal ValueComments
Drying Temperature 150 °C
Dry Time 3.00 hour
 
Descriptive Properties
Colornatural
Fiber volume content (%)50
General material information0.31 mmply thickness (consolidated)
 1000 mmMaterial widths
 1270 mmMaterial widths
 280 g/m²Fiber areal weight
 482 g/m²Areal weight finished product
 atlas 5HSFiber architecture
 carbon HT 3kFiber type
Resin weight content (%)41.9

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENSIN8245 / 319173

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.