Notes: Ultra pure VMQ with very good mechanical properties for food, drinking water and medical applications Approvals: - 3 3-A Sanitary Standard Number 18-03 Class I
- ADI free
- BfR XV (Silicone)
- Dlgs. 25.01.1992 n.108 Art. 2 Parte D
- D.M. 21/03/1973
- DVGW W 270
- EC 1935/2004 article 3
- FDA - CFR 21 - 177.2600 food a) - f)
- French Arrêté 25/11/1992 (migration test)
- GB 4806.1-2016
- GB 4806.11-2016
- GB 9685-2016
- GMC/RES. No. 28/99
- KIWA NSF/ANSI 51formulation
- KTW Guideline cold water (23 °C) and hot water (85 °C)
- LFGB § 30/31
- Phthalate free
- SR 817.023.21
- USP Class VI chapter 87 and 88, 121°C
- DVGW EN 549 D2/H3
- PAH Category 1 (AfPS GS 2014:01)
- PAHs requirements acc. Regulation (EU) No 1272/2013
Information provided by Angst + Pfister |