MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Go Yen Chemical GOYENCHEM-AA32 Anti-Ozonant
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: CAS No.6600-31-3

Intro: Since the olefin content of rubber compound is vulnerable to ozone attack, and it will cause the rubber, tires and all kinds of products get aging and brittleness. So, the tire is very easy to cause a blowout which leads to personal injury or even death. GOYENCHEM-AA32 made by GO YEN CHEMICAL INDUSTRIAL CO., LTD. (GYC GROUP) which is a perfect solution to protect rubber and tire from ozone attack and ensures a neat appearance. GOYENCHEM-AA32 it is an effective, non-discoloring and non-standing anti-ozonant. Moreover, this product is equivalents as LANXESS AFS/LG. It also supplies the high value for products and the world’s famous rubber and tires company designated product.

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 - 1.26 g/cc0.0397 - 0.0455 lb/in³
Volatiles <= 0.20 %<= 0.20 %
 
Thermal PropertiesMetricEnglishComments
Melting Point 85.9 - 95.9 °C187 - 205 °F
Boiling Point 436.7 - 446.7 °C818.1 - 836.1 °F
 
Descriptive Properties
AppearancePowder
ColorOdorless
Solubility0.5g in 100 ml Cyclohexane
 1.73 mg/Lg in 100 ml Water
 10g in 100 ml Toluene
 43g in 100 ml Acetone

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOYEN366 / 266674

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.