MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Specialty Materials 5521-F Boron Epoxy Prepreg Tape
Categories: Polymer; Thermoset; Epoxy

Material Notes: Specialty Materials' 5521-f is a highly advanced prepreg tape with boron fibers in an a tough, rigid, 250°F curing epoxy resin.It is a 6-in. wide one-step tape, laminated resin films and scrim cloth with creeled fibers collimated at 208/inch (4-mil) or 152/inch (5.6-mil).

Property data reported for samples with 4 mil fiber.

Information provided by Specialty Materials, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.00 g/cc0.0723 lb/in³
Thickness 130 microns5.12 milcured ply
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 1520 MPa220000 psi
Modulus of Elasticity 185 GPa26800 ksi
Flexural Yield Strength 1790 MPa260000 psi
Flexural Modulus 190 GPa27600 ksi
Compressive Yield Strength 2930 MPa425000 psi
Compressive Modulus 210 GPa30500 ksi
Poissons Ratio 0.210.21
Shear Strength 97.0 MPa14100 psiInterlaminar
 
Processing PropertiesMetricEnglishComments
Processing Temperature 121 °C250 °FCure Temp.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSPEC00f / 287751

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.