MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Radici RADILON® MIXLOY S 32HSA20K 100 NT PA6/ABS Blend, Heat Stabilized, Dry
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend

Material Notes: Description: PA6/ABS blend, medium viscosity extrusion grade. Heat stabilized. Natural color. Suitable for parts requiring low moisture absorption and high dimensional stability. Also apt for 3D printing

Processing: 3D Printing, Profile Extrusion, Other Extrusion

Delivery Form: Granules

Additives: Lubricants, Release agent

Special Characteristics: Heat stabilized or stable to heat, Amorphous, Improved Dimensional Stability, High Surface Aspect, Low Moisture Absorption

Industries: Automotive, Consumer Industry Goods, Transportation

Regional Availability: North America, Europe, Asia Pacific, South and Central America, Near East/Africa

Information provided by Radici Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.09 g/ccISO 1183
Water Absorption 6.4 %
@Thickness 2.00 mm
Immersion at 23°C; ISO 62
Moisture Absorption 2.00 %
@Thickness 2.00 mm
50% RH; ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 60.0 MPa50 mm/min; ISO 527-2/1A
Elongation at Break >= 50 %Nominal, 50 mm/min; ISO 527-2/1A
Elongation at Yield 4.0 %50 mm/min; ISO 527-2/1A
Tensile Modulus 2500 MPa1mm/min; ISO 527-2/1A
Flexural Strength 90.0 MPa2mm/min; ISO 178
Flexural Modulus 2500 MPa2mm/min; ISO 178
Charpy Impact Unnotched NBISO 179/1eU
Charpy Impact, Notched 9.00 kJ/m²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 220 °CISO 11357-1/-3
Vicat Softening Point 130 °C
@Load 5.10 kg
50°C/h; ISO 306
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 260 °C
Middle Barrel Temperature 260 °CCenter Rear
 265 °CCenter Front
Front Barrel Temperature 270 °C
Melt Temperature 275 °C
Head Temperature 275 °CHead and Die

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PRADICI103 / 313604

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.