MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Toyobo Riteflex® 100CB Thermoplastic Copolyester Elastomer
Categories: Polymer; Thermoplastic; Polyester, TP; Polyester Thermoplastic Elastomer

Material Notes: Product Description: Riteflex 100CB is a carbon black masterbatch concentrate designed to provide black color to natural Riteflex TPC-ET grades. Typical let-down ratio is 1:40. Riteflex 100CB can be added to natural Riteflex TPC-ET grades with our without other Riteflex masterbatches like Riteflex 102UV and/or Riteflex 102HS. Riteflex masterbatches are specially designed to provide certain features to natural Riteflex grades with minimal effect on performance properties. Riteflex masterbatches should be blended with Riteflex natural grades prior to use – they are not intended to be used directly for manufacturing of parts.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Uses: Color Concentrates

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80
@Time 15.0 sec
ISO 868
Resilience 65ASTM D2632
Tear Strength 428 pliISO 34-1
 428 pliFlow, Die C; ISO 34-1
 
Thermal PropertiesOriginal ValueComments
Melting Point 338 °F
 
Processing PropertiesOriginal ValueComments
Feed Temperature 311 - 338 °FInjection
Zone 4 338 - 356 °FInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHCQ6313 / 311006

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.