System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
SABIC LNP™ THERMOCOMP™ Compound EF006 Polyetherimide (PEI) (Europe)
Categories:
Polymer
;
Thermoplastic
;
Polyetherimide (PEI)
Material Notes:
LNP THERMOCOMP EF006 compound is based on Polyetherimide (PEI) resin containing 30% glass fiber.
Features: High Stiffness,High Heat Resistance,Structural
Information provided by SABIC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.52
g/cc
ISO 1183
Moisture Absorption
0.0200 %
Injection Molding
Linear Mold Shrinkage, Flow
0.0020
-
0.0040
cm/cm
SABIC method
Mechanical Properties
Original Value
Comments
Tensile Strength, Yield
169
MPa
5 mm/min; ISO 527
Elongation at Break
2.0 %
5 mm/min; ISO 527
Tensile Modulus
10350
MPa
1 mm/min; ISO 527
Flexural Strength
235
MPa
yield, 2 mm/min; ISO 178
Flexural Modulus
9200
MPa
2 mm/min; ISO 178
Izod Impact, Notched (ISO)
10.0
kJ/m²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO)
45.0
kJ/m²
80*10*4; ISO 180/1U
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
18.0
µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow
43.0
µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi)
214
°C
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi)
209
°C
Flatw 80*10*4 sp=64mm; ISO 75/Af
UL RTI, Electrical
105
°C
UL 746B
UL RTI, Mechanical with Impact
105
°C
UL 746B
UL RTI, Mechanical without Impact
105
°C
UL 746B
Flammability, UL94
V-0
@Thickness >=0.750 mm
UL 94
Processing Properties
Original Value
Comments
Nozzle Temperature
390
-
400
°C
Zone 2
370
-
390
°C
Zone 3
380
-
400
°C
Melt Temperature
360
-
400
°C
Injection Molding
Mold Temperature
140
-
180
°C
Drying Temperature
150
°C
Injection Molding
Dry Time
4.00
-
6.00
hour
Injection Molding
Back Pressure
0.300
-
0.700
MPa
Vent Depth
0.00250
-
0.00760
cm
Descriptive Properties
Screw speed (Circumferential speed)
0.2-0.3 m/s
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PSABH81590 / 289537
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.