MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SACO AEI PEXIDAN® V/T-2 Curable Polyethylene Compound
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Low Density, Moisture Curable Polyethylene Compound, for Low Voltage Building Wire, Control Cable and Cable Tray Applications (UL Styles SIS, XHH, XHHW, XHHW-2, RHH, RHW, and RHW-2 VW-1). Also CSA listed for RW-90 and CIC (-40C rated).

PEXIDAN® V/T-2 is a low density flame-retardant XLPE system curable by moisture and consists of a silane-grafted base compound A-3001 and a catalyst masterbatch CAT-045FR. Mixed and extruded in the proper proportions (50/50), the two components result in a material that is curable by exposure to hot water. PEXIDAN® V/T-2 is halogenated but is RoHS compliant.

Information provided by SACO AEI Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.32 g/ccASTM D792
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Deformation 5.0 %UL 1581 / UL 2556
Storage Temperature <= 30.0 °F
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 2200 psiUL 1581 / UL 2556
 2100 psi
@Temperature 23.0 °C
30 day gasoline; UL 1581 / UL 2556
 2200 psi
@Temperature 75.0 °C
60 day oil; UL 1581 / UL 2556
 2400 psi
@Temperature 121 °C,
Time 605000 sec
after thermal ageing; UL 1581 / UL 2556
Elongation at Break 400 %UL 1581 / UL 2556
 375 %
@Temperature 23.0 °C
30 day gasoline; UL 1581 / UL 2556
 400 %
@Temperature 75.0 °C
60 day oil; UL 1581 / UL 2556
 45 %
@Temperature 150 °C,
Time 900 sec
Hot, Elongation under 0.2 N/mm2 load; SACO AEI DWI-QA-4007 based on ICEA T-28-562
 400 %
@Temperature 121 °C,
Time 605000 sec
after thermal ageing; UL 1581 / UL 2556
Crush Resistance 1290 lb (mass)UL 1581 / UL 2556
 
Electrical PropertiesOriginal ValueComments
Insulation Resistivity 3.60e+6 Megaohm/1000 ft
@Temperature 90.0 °C
After 12 weeks; CSA C22.2 No. 38 UL 44
 6.10e+6 Megaohm/1000 ft
@Temperature 90.0 °C
CSA C22.2 No. 38 UL 44
 1.00e+7 Megaohm/1000 ft
@Temperature 15.0 °C
CSA C22.2 No. 38 UL 44
Dielectric Constant 3.1
@Temperature 90.0 °C
UL 1581 / UL 2556
 2.56
@Frequency 1.00e+6 - 1.00e+8 Hz
ASTM D150
Dielectric Breakdown 11000 VAfter glancing impact; UL 1581 / UL 2556
 36000 VUL 1581 / UL 2556
Dissipation Factor 0.00094
@Frequency 1e+8 Hz
ASTM D150
 0.00232
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -60.0 °CLTBP; ASTM D746
Oxygen Index 27 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Processing Temperature 310 - 340 °Fbarrel zones
Die Temperature 365 °F
Head Temperature 365 °F
 
Descriptive Properties
Degree of Crosslinking60%ASTM D2765
FV-2 / VW-1 Flame TestPassUL 1581 / UL 2556

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSACO052 / 249419

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.