MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Konson DPG-80 Masterbatch
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Composition: 80% N,N'-diphenyl guanidine based on specification, 20% EPDM binder and dispersing agents

Use Characteristics: The curing accelerator Konson® DPG-80 gives a very long scorch time and a relatively slow full cure. It causes slight discolouration and cannot be used in light-coloured articles, except as an activator. When Konson® DPG-80 is used on its own the resistance of the vulcanizates to hot air and oxygen is poor (requiring the use of effective antioxidants). Accelerators of the mercapto type are strongly activates by Konson® DPG-80. In IIR and EPDM compounds, Konson® DPG-80 has only little effect.

Processing Advantages: The thermoplastic, excellent compatible EPDM/EVA binder which is combined with active dispersing promoters allows much more easy quickly incorporation and excellent dispersion in the rubber mixing. In this way, optimal activity of the effective CBS is assured.

Dosage levels: primary: 1 - 2 phr with 2,5 - 3,5 phr sulphur; secondary: 0,1 - 0,25 phr with 0,75 - 1 phr mercapto accelerator and 2,5 phr sulphur.

Applications: Automotive and construction profile, Tire treads, air hoses, conveyor belts, footwear and other technical articles.

Information provided by Konson®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.09 - 1.15 g/cc
Ash <= 0.40 %
Evaporation Loss <= 0.30 %
 
Thermal PropertiesOriginal ValueComments
Melting Point 144 °C
 
Descriptive Properties
Active content= 96%
AppearanceWhite or grey-white granules
Sieve residue= 0.1 %63µm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKONS015 / 256060

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.