MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultradur® S 4090 G4 BK15051 PBT/ASA, 20% Glass Reinforced
Categories: Polymer; Thermoplastic; ASA Polymer; Polyester, TP; Polybutylene Terephthalate (PBT); PBT + ASA Blend, Glass Fiber Reinforced

Material Notes: Ultradur S 4090 G4 BK15051 is a 20% glass reinforced, pigmented black PBT+ASA blend. It produces moldings with good surface finish, is resistant to chemicals and stress cracking, and has low shrinkage and warpage.

Applications: Applications include highly stressed equipment housings in the automotive, electrical and household sectors.

Information provided by BASF.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.38 g/cc0.0499 lb/in³ISO 1183
Moisture Absorption 0.200 %0.200 %50% RH; ISO 62
Water Absorption at Saturation 0.40 %0.40 %ISO 62
Viscosity Test 108 cm³/g1.08 dl/gISO 1628
Melt Flow 14.7 g/10 min
@Load 2.16 kg,
Temperature 275 °C
14.7 g/10 min
@Load 4.76 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 108 MPa15700 psiISO 527
Elongation at Yield 2.4 %2.4 %ISO 527
Tensile Modulus 7.00 GPa1020 ksiISO 527
Flexural Modulus 6.40 GPa928 ksiISO 178
Charpy Impact, Notched 0.700 J/cm²3.33 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 40.0 µm/m-°C22.2 µin/in-°F
Melting Point 223 °C433 °FISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 184 °C363 °FISO 75
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 - 270 °C482 - 518 °F
Mold Temperature 60.0 - 100 °C140 - 212 °F
Drying Temperature 100 - 120 °C
@Time 14400 sec
212 - 248 °F
@Time 4.00 hour
Moisture Content <= 0.040 %<= 0.040 %
Injection Pressure 3.45 - 10.3 MPa500 - 1500 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASF8915 / 254873

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.