System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
SABIC CYCOLOY™ FR CY6414 PC+ABS (Europe)
Categories:
Polymer
;
Thermoplastic
;
ABS Polymer
;
Polycarbonate/ABS Alloy, Unreinforced
Material Notes:
CYCOLOY CY6414 is an impact modified PC blend, medium flow and high heat resistant, injection moldable, non chlorinated/brominated flame retardant grade. It has a UL94 V0@1.2mm and 5VB@2.5mm flame rating.
Information provided by SABIC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.18
g/cc
ISO 1183
Water Absorption
0.30 %
23°C/sat; ISO 62
Moisture Absorption
0.100 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow
0.0040
-
0.0080
cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow
13
g/10 min
@Load 5.00 kg,
Temperature 260 °C
cm³/10 min; ISO 1133
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
62.0
MPa
50 mm/min; ASTM D638
67.0
MPa
50 mm/min; ISO 527
Tensile Strength, Yield
64.0
MPa
50 mm/min; ASTM D638
66.0
MPa
50 mm/min; ISO 527
Elongation at Break
85 %
50 mm/min; ASTM D638
>= 100 %
50mm/min; ISO 527
Elongation at Yield
5.7 %
50 mm/min; ISO 527
6.0 %
50 mm/min; ASTM D638
Tensile Modulus
2330
MPa
5 mm/min; ASTM D638
2420
MPa
1mm/min; ISO 527
Flexural Yield Strength
96.0
MPa
2 mm/min; ISO 178
Flexural Modulus
2470
MPa
2 mm/min; ISO 178
Izod Impact, Notched (ISO)
50.0
kJ/m²
80*10*4; ISO 180/1A
12.0
kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO)
NB
80*10*4; ISO 180/1U
NB
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Charpy Impact Unnotched
NB
Edgew 80*10*4 sp=62mm; ISO 179/1eU
NB
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched
20.0
kJ/m²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
12.0
kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Electrical Properties
Original Value
Comments
Volume Resistivity
1.00e+15
ohm-cm
IEC 60093
Surface Resistance
4.00e+16
ohm
ROA; IEC 60093
Dielectric Constant
2.95
@Frequency 1e+6 Hz
ASTM D150
3.01
@Frequency 1000 Hz
ASTM D150
Dissipation Factor
0.0017
@Frequency 1000 Hz
ASTM D150
0.0088
@Frequency 1e+6 Hz
ASTM D150
0.0088
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index
175
-
250
V
UL 746A
Hot Wire Ignition, HWI
30
-
60
sec
UL 746A
High Amp Arc Ignition, HAI
60
-
120
arcs
UL 746A
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
70.0
µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow
70.0
µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Hot Ball Pressure Test
125
°C
IEC 60695-10-2
125
°C
IEC 60695-10-2
Deflection Temperature at 1.8 MPa (264 psi)
116
°C
Flatw 80*10*4 sp=64mm; ISO 75/Af
118
°C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point
133
°C
Rate B/50; ISO 306
134
°C
Rate B/120; ISO 306
UL RTI, Electrical
105
°C
UL 746B
UL RTI, Mechanical with Impact
95.0
°C
UL 746B
UL RTI, Mechanical without Impact
100
°C
UL 746B
Flammability, UL94
V-0
@Thickness 1.20 mm
UL 94
5VB
@Thickness 2.50 mm
UL 94
Oxygen Index
32 %
ISO 4589
Glow Wire Test
775
°C
@Thickness 3.00 mm
IEC 60695-2-13
775
°C
@Thickness 0.750 mm
IEC 60695-2-13
775
°C
@Thickness 1.50 mm
IEC 60695-2-13
960
°C
@Thickness 0.750 mm
IEC 60695-2-12
Processing Properties
Original Value
Comments
Processing Temperature
60.0
-
80.0
°C
Hopper Temperature
Nozzle Temperature
230
-
290
°C
Injection Molding
Zone 1
210
-
260
°C
Zone 2
230
-
290
°C
Zone 3
240
-
300
°C
Melt Temperature
250
-
300
°C
Mold Temperature
60.0
-
90.0
°C
Drying Temperature
90.0
-
100
°C
Injection Molding
Dry Time
2.00
-
4.00
hour
Injection Molding
Moisture Content
0.020 %
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PSABI10804 / 244271
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.