MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis BorSafe™ HE3497-LS-H HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: BorSafe HE3497-LS-H is a bimodal polyethylene compound produced by the advanced Borstar technology. The product is a readymade compound, including carefully selected stabilizers to ensure excellent long-term thermal stability and UV-resistance for limited outdoors storage of the final product. Furthermore, it has a pigment system that gives a bright colored stripe, even when extruded as a thin layer on a black pipe.

Applications:

  • Industrial applications
  • Waste water discharge
  • Pressure sewerage
BorSafe HE3497-LS-H is recommended to extrude identification stripes onto black pipes produced from BorSafe materials. The compound used for the identification stripes is manufactured from a PE BorSafe base polymer for which fusion compatibility has been proven according to part 1 of the EN and ISO PE pressure pipe standards. The resistance to weathering of the identification stripe compound as a cumulative radiant exposure is > 7 GJ/m² related to the outdoor storage ability limit as the base resin already fulfills this requirement.

Specifications: BorSafe" HE3497-LS-H and/or articles produced from it, are expected to meet the applicable requirements included in the below mentioned standards provided it is processed using sound material handling and processing practices as well as appropriate testing procedures. EN 12201; ISO 4427

Thanks to the molecular structure selected, BorSafe HE3497-LS-H offers outstanding extrudability and an easy application of the thin co-extruded stripes onto the black core pipe. The red-brown color is similar to color code RAL 8023.

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.9565 g/cc0.03456 lb/in³ISO 1183-1/Method A
Oxidative Induction Time (OIT) >= 20.0 min
@Temperature 210 °C
>= 20.0 min
@Temperature 410 °F
ISO 11357-6
Melt Flow 0.300 g/10 min
@Load 5.00 kg,
Temperature 190 °C
0.300 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133-1
Storage Temperature <= 50.0 °C<= 122 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 190 - 210 °C374 - 410 °FCylinder
Melt Temperature 200 - 220 °C392 - 428 °F
Shelf Life 36.0 Month36.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBORE9666 / 323023

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.