MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
SABIC LNP™ THERMOTUF™ Compound DF008EI Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP THERMOTUF DF008EI compound is based on Polycarbonate (PC) resin containing 40% glass fiber. Added features of this grade include: Easy Molding, Impact Modified.

Features: Impact Modified,High Stiffness,Easy Molding,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.51 g/ccASTM D792
 1.51 g/ccISO 1183
Moisture Absorption 0.0200 %Injection Molding
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.0020 - 0.0040 cm/cm24hrs; ISO 294
 0.0030 cm/cm24hrs; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 130 MPaISO 527
 132 MPaASTM D638
Tensile Strength, Yield 129 MPaISO 527
 132 MPaASTM D638
Elongation at Break 2.0 %ISO 527
 2.2 %ASTM D638
Elongation at Yield 2.0 %ISO 527
 2.2 %ASTM D638
Tensile Modulus 11060 MPa1 mm/min; ISO 527
 12630 MPa50 mm/min; ASTM D638
Flexural Strength 140 MPaISO 178
 199 MPaASTM D790
Flexural Modulus 10090 MPaISO 178
 10610 MPaASTM D790
Izod Impact Notched 160 JASTM D256
Izod Impact, Unnotched 838 J/mASTM D4812
Izod Impact, Notched (ISO) 16.0 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 51.0 kJ/m²80*10*4; ISO 180/1U
Dart Drop, Total Energy 23.0 Jpeak; ASTM D3763
Impact Test 7.00 JMultiaxial Impact; ISO 6603
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 25.2 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 26.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 41.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 42.5 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 135 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 133 °C
@Thickness 3.20 mm
unannealed; ASTM D648
UL RTI, Electrical 80.0 °CUL 746B
UL RTI, Mechanical with Impact 80.0 °CUL 746B
UL RTI, Mechanical without Impact 80.0 °CUL 746B
Flammability, UL94 HB
@Thickness >=0.400 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Zone 2 310 - 320 °C
Zone 3 320 - 330 °C
Melt Temperature 305 - 325 °CInjection Molding
Mold Temperature 80.0 - 110 °C
Drying Temperature 120 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH81997 / 289944

Ensinger SPI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.