MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Amodel® A-4422 LS WH118 Polyphthalamide (PPA), 22% Mineral  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), Mineral Filled

Material Notes: Amodel® A-4422 LS resin is a 22% reinforced, light-stabilized, high-reflectivity white grade of polyphthalamide (PPA). The material exhibits high heat resistance, high strength and stiffness over a broad temperature range, low moisture absorption, excellent chemical resistance, and excellent electrical properties.

Its rapid crystallization rate and high flow characteristics can result in shorter cycles, thereby enhancing molding productivity and lowering costs.

- White: A-4422 LS WH118

Chemical Resistant; Fast Molding Cycle; Good Color Stability; High Reflectivity; High Stiffness; Light Stabilized; Low Moisture Absorption

Uses: Automotive Applications; Automotive Electronics; LEDs

Processing: Injection Molding

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.60 g/ccMethod A; ISO 1183
 1.60 g/ccMethod A; ISO 1183
Water Absorption 0.20 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.0060 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 102 MPaASTM D638
Elongation at Break 1.3 %ISO 527-2
Tensile Modulus 9100 MPaISO 527-2
Flexural Strength 171 MPaISO 178
Flexural Modulus 7790 MPaISO 178
Izod Impact, Notched (ISO) 2.90 kJ/m²Type 1, Notch A; ISO 180
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 31.0 µm/m-°C
@Temperature 200 - 250 °C
ASTM E831
 31.0 µm/m-°C
@Temperature 50.0 - 100 °C
ASTM E831
 938 µm/m-°C
@Temperature 100 - 150 °C
ASTM E831
CTE, linear, Transverse to Flow 63.0 µm/m-°C
@Temperature 50.0 - 100 °C
ASTM E831
 100 µm/m-°C
@Temperature 100 - 150 °C
ASTM E831
 150 µm/m-°C
@Temperature 200 - 250 °C
ASTM E831
Melting Point 324 °CISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 306 °CUnannealed; ISO 75-2/B
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 318 - 324 °C
Front Barrel Temperature 327 - 332 °C
Melt Temperature 329 - 343 °C
Mold Temperature 66.0 - 93.0 °C
Drying Temperature 120 °C
@Time 14400 sec
Moisture Content 0.045 %
 
Descriptive Properties
ColorWhite
FormsPellets
RoHS ComplianceRoHS Compliant

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Zytel® HTNFE8200 NC010 PA6T/XT-HI
Celanese Zytel® HTN51G35HSL NC010 PA6T/XT-GF35
Celanese Zytel® HTN51G35EF BK083 PA6T/XT-GF35
High Strength Modified Copper, UNS C19400, O82 Temper flat products
High Strength Modified Copper, UNS C19400, O60 Temper flat products

PSOL8Y6052 / 192973

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.