MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
HB Fuller AT-3 Very High Bond Acrylic Tape
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: AT-3 is a pressure sensitive, structural grade, solid acrylic tape system designed to provide a superior bond between a wide variety of substrates. The tape possesses a uniform, high-tack, acrylic adhesive on both surfaces with an integral core of solid acrylic polymer and will bond to most clean, dry, oil-free substrates. Thickness ranges from 0.64mm to 2mm (0.025” to 0.080”)Width ranges from 6mm to 457mm (0.25” to 18”)

AT-3 offers numerous advantages including a waterproof bond, ease of application, and the ability to withstand thermal movement.

Features and Benefits:

  • Pressure sensitive bonding
  • Solid composition for easy cutting
  • Moisture resistant
  • Excellent weathering properties
  • Maintains adhesion at sub-zero temperatures
  • Hardening or brittle resistant with age
  • Flexible – conforms to intricate shapes

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Storage Temperature 4.00 - 38.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 2.20 MPaASTM D412 Die C
Elongation at Break 500 %ASTM D412 Die C
Shear Strength 0.620 MPaDynamic; ASTM D3164
Peel Strength 0.0290 pli90° Peel Adhesion; ASTM D3330
 0.0590 pliChemical Resistance - Cleavage Peel, Diesel Fuel - 1hr; FLTM BU 112-02, Method C
 0.0620 pliChemical Resistance - Cleavage Peel, Water Immersion - 240hrs; FLTM BU 112-02, Method C
 0.0730 pliChemical Resistance - Cleavage Peel, Unleaded Gasoline - 1hr; FLTM BU 112-02, Method C
 0.0860 pliChemical Resistance - Cleavage Peel, 3 Days @ RT; FLTM BU 112-02, Method C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 93.0 °C
Minimum Service Temperature, Air -34.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 34.0 Month
 
Descriptive Properties
ColorTranslucent
ConsistencyTape

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHBFULL157 / 316948

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.