MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Angst+Pfister APSOplast® PF CP MF Special laminated paper, MKHP
Categories: Polymer; Thermoset

Material Notes: (phenolic resin/cellulose paper + melamine resin composite laminate material)

This special laminated paper is coated with a 0.3 mm layer of melamine resin on both sides. It has extremely high track resistance and dielectric strength, is scratch-resistant and gen erally resistance to chemicals. This material can easily be labeled, printed, laminated and is flame-retardant.

Information provided by Angst + Pfister

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.40 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 120 MPaISO 527
Modulus of Elasticity 16.0 GPaflexural test; ISO 178
Flexural Strength 140 MPaISO 178
Compressive Strength 250 MParesistance, perpendicular to layers; ISO 604
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1.00e+9 ohmafter 24 h immersed in water; IEC 60167
Dielectric Constant 5.0DIN 53483
Dielectric Strength 10.0 kV/mmat 90°C in oil parallel to layers; IEC 60243-1
Dielectric Loss Index 0.080after 24 h immersed in water; DIN 53483
Comparative Tracking Index 600 V[kV], at 90°C in oil parallel to layers; IEC 60243-1
 
Thermal PropertiesOriginal ValueComments
CTE, linear 20.0 - 40.0 µm/m-°CVDE 0304/2
Thermal Conductivity 0.200 W/m-KDIN 52612
 
Descriptive Properties
Colorlight grey (RAL 7035)
Disruptive discharge voltage30
Water Absorption200[mg], 10 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PANGP097 / 250595

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.