MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
TSRC T-BLEND® 1500-70N TPR/TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: T-BLEND® is a series of thermoplastic elastomer compound materials produced by TSRC Corporation. T-BLEND® 1500-70Nis specifically designed for medical film ,Mainly used in medical drapes, medical cover film, and other disposable medical treatment of the application of the film, and can be used to replace the traditional TPU, PVC products. T-BLEND® 1500-70N is embedded period of polystyrene Copolymer (SBC, Styrenic Block Copolymer) for the base blend. T-BLEND® 1500-70N Can be recovery processing, gate, port and waste plastic materials can be processed to use.

Information provided by TSRC Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.910 - 0.950 g/ccASTM D792
Melt Flow 6.0 - 14 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 67 - 73ASTM D2240
Tensile Strength 50.0 kg(f)/cm²Type3, specimen; ASTM D412
Elongation at Break 800 %Crosshead; ASTM D412
300% Modulus 25.0 kg(f)/cm²500mm/min; ASTM D412
Tear Strength 25.0 kg(f)/cmC Die; ASTM D624
 
Processing PropertiesOriginal ValueComments
Feed Temperature 190 °C
Rear Barrel Temperature 180 - 200 °C
Front Barrel Temperature 200 - 210 °C
Die Temperature 160 - 200 °C
Drying Temperature 70.0 °C
@Time 3600 - 7200 sec
hot air circulating oven/hopper
 
Descriptive Properties
ColorBlue
FormPellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTSRC046 / 306334

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.