BorShape™ FX1003 is a high alpha olefin terpolymer polyethylene blown film grade made with proprietary Borealis Borstar® 3G Technology combining unprecedented process ability together with outstanding stiffness/toughness balance. BorShape FX1003 outstanding mechanical performance allows further downgauging in flexible packaging but also support maximization of Post Consumer recycled polyethylene content leading to increased sustainability of the final packaging. CAS No. 60785-11-7 Applications: - Flexible packaging
- Collation shrink
- Heavy-duty bags
- Medium duty bags
- Frozen food packaging
- Form fill and seal film
- MDO film (Monomaterial solution)
- Non food contact film with high content of Post Consumer
- Recycled
Additives: BorShape FX1003 contains antioxidant. Special Features: BorShape FX1003 allows high Post Consumer Recycled incorporation in non food contact application without thickness increase. BorShape FX1003 is ideally used as stiffness provider together with NAV101 and/or CWT100LG Post Consumer Recycled Low Density Polyethylene in high end transparent non food contact applications. BorShape FX1003 tailor-made design makes the material perfectly suited for MDO process. Information provided by Borealis AG |