MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Master Bond MasterSil 711Med One Component Medical Grade Silicone Adhesive
Categories: Polymer; Thermoset; Silicone

Material Notes: Key Features:
  • Ultra fast and non-corrosive cure
  • Outstanding electrical insulation properties
  • Bonds well to a wide variety of substrates
  • Conveniently packaged in 30 cc syringes
  • Good sterilization resistance
  • Meets ISO 10993-5 certification
Product Description: MasterSil 711Med is an easy to use, one component, high performance silicone elastomer compound for bonding, sealing, coating and formed-in-place gaskets. This specialty system is most noteworthy for its very fast and completely non-corrosive cure. MasterSil 711Med is flowable and bonds well to a broad range of substrates, including glass, metals and many plastics. The speed of the cure depends on the thickness of the layer and the humidity; the thinner the layer the faster the cure. It is extremely soft with superb flexibility and elasticity and outstanding electrical insulation properties. The system is resistant to many sterilants including EtO, gamma, radiation, glutaraldehyde and other liquid steriliants. MasterSil 711Med is translucent. It is serviceable from -75°F to +400°F. One particularly useful product property is its ability to adhere well to silicone substrates, a commonly used material in medical device manufacturing. Moreover, since the system is totally non-corrosive, it is compatible for medical electronic applications. These special product properties enable the system to be a candidate in a number of different medical device manufacturing situations.

Information provided by Master Bond, Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/cc
Viscosity 60000 - 80000 cP60000 - 80000 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 25.0 - 35.025.0 - 35.0
Tensile Strength 2.76 - 3.45 MPa400 - 500 psi
Elongation at Break 300 - 400 %300 - 400 %
Adhesive Bond Strength 1.38 - 1.72 MPa200 - 250 psilap shear, aluminum to aluminum
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cm
Dielectric Constant 2.50
@Frequency 60 Hz
2.50
@Frequency 60 Hz
Dielectric Strength 19.7 kV/mm
@Thickness 3.17 mm
500 kV/in
@Thickness 0.125 in
Dissipation Factor 0.00300
@Frequency 60 Hz
0.00300
@Frequency 60 Hz
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 204 °C399 °F
Minimum Service Temperature, Air -59.0 °C-74.2 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 2.00 - 5.00 min0.0333 - 0.0833 hourTack-free time, >50% humidity
Shelf Life 6.00 Month6.00 Monthin original, unopened containers
 
Descriptive Properties
ColorTranslucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMASTM5808 / 323325

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.