MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC LNP™ FARADEX™ Compound AS002 Acrylonitrile Butadiene Styrene (ABS)
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: LNP FARADEX AS002 compound is based on Acrylonitrile Butadiene Styrene (ABS) resin containing 10% stainless steel fiber. Added features of this grade include: Electrically Conductive, EMI/RFI shielding.

Features: EMI/RFI Shielding,Electrically Conductive

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.11 g/cc0.0401 lb/in³ISO 1183
 1.12 g/cc0.0405 lb/in³ASTM D792
Moisture Absorption 0.0500 - 0.100 %0.0500 - 0.100 %Injection Molding
 0.200 %0.200 %23°C/50% RH/24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0018 cm/cm0.0018 in/in24hrs; ASTM D955
 0.0018 cm/cm0.0018 in/in24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.0027 cm/cm0.0027 in/in24hrs; ASTM D955
 0.0027 cm/cm0.0027 in/in24hrs; ISO 294
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 37.0 MPa5370 psiISO 527
 39.0 MPa5660 psiASTM D638
Tensile Strength, Yield 39.0 MPa5660 psiISO 527
 42.0 MPa6090 psiASTM D638
Elongation at Break 3.3 %3.3 %ISO 527
 8.6 %8.6 %ASTM D638
Elongation at Yield 2.2 %2.2 %ASTM D638
 2.2 %2.2 %ISO 527
Tensile Modulus 2.50 GPa363 ksi1 mm/min; ISO 527
 2.99 GPa434 ksi50 mm/min; ASTM D638
Flexural Strength 66.0 MPa9570 psiISO 178
 75.0 MPa10900 psiASTM D790
Flexural Modulus 2.50 GPa363 ksiISO 178
 2.81 GPa408 ksiASTM D790
Izod Impact Notched 58.0 J42.8 ft-lbASTM D256
Izod Impact, Unnotched 2.86 J/cm5.36 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 7.00 kJ/m²3.33 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 20.0 kJ/m²9.52 ft-lb/in²80*10*4; ISO 180/1U
Dart Drop, Total Energy 11.0 J8.11 ft-lbpeak; ASTM D3763
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 100 - 1.00e+6 ohm-cm100 - 1.00e+6 ohm-cmASTM D257
Surface Resistance 10 ohm - 1e+0510 ohm - 1e+05ASTM D257
Shielding Effectiveness 40 - 55 dB
@Thickness 3.00 mm
40 - 55 dB
@Thickness 0.118 in
SABIC method
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  78.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
43.3 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
 79.2 µm/m-°C
@Temperature -40.0 - 40.0 °C
44.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
CTE, linear, Transverse to Flow  75.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
42.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 96.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
53.3 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 91.0 °C196 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 97.0 °C
@Thickness 3.20 mm
207 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °C172 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 87.0 °C
@Thickness 3.20 mm
189 °F
@Thickness 0.126 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Zone 2 230 - 245 °C446 - 473 °F
Zone 3 255 - 265 °C491 - 509 °F
Melt Temperature 240 - 255 °C464 - 491 °FInjection Molding
Mold Temperature 70.0 - 95.0 °C158 - 203 °F
Drying Temperature 80.0 °C176 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80622 / 288569

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.