MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Teknor Apex Monprene® MP-1500 Thermoplastic Elastomer  (Unverified Data**)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene MP-1500 is a thermoplastic elastomer designed specifically for the consumer market. Monprene MP-1500 is a clear, medium hardness grade low density, medium hardness grade that exhibits low compression set, good abrasion and chemical resistance, and is suitable for injection molding and extrusion.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Abrasion Resistant; Chemical Resistant; Good Colorability; Good Melt Strength; Good Tear Strength; Low Compression Set; Weather Resistant

Uses: Consumer Applications; Gaskets; Handles; Household Goods; Kitchenware; Outdoor Applications; Packaging; Rubber Replacement; Safety Equipment; Strain Reliefs; White Goods & Small Appliances; Writing Instruments

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Extrusion; Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.892 g/ccASTM D792
Melt Flow 1.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 65ASTM D2240
 63
@Time 5.00 sec
ASTM D2240
Tensile Strength at Break 2150 psiASTM D412
Tensile Stress at Strain 339 psi
@Strain 100 %
ASTM D412
 444 psi
@Strain 200 %
ASTM D412
 576 psi
@Strain 300 %
ASTM D412
Elongation at Break 730 %ASTM D412
Tear Strength 188 pli20 in/min, Across Flow; ASTM D624
 192 pli20 in/min, Flow; ASTM D624
Compression Set 11 %
@Temperature 22.8 °C,
Time 79200 sec
ASTM D395
 
Processing PropertiesOriginal ValueComments
Processing Temperature 390 - 480 °FMelt, Injection
Rear Barrel Temperature 360 - 450 °FInjection
Middle Barrel Temperature 370 - 460 °FInjection
Front Barrel Temperature 380 - 470 °FInjection
Nozzle Temperature 390 - 480 °FInjection
Zone 1 360 - 450 °FExtrusion
Zone 2 370 - 460 °FExtrusion
Zone 3 380 - 470 °FExtrusion
Zone 4 380 - 470 °FExtrusion
Zone 5 390 - 480 °FExtrusion
Die Temperature 390 - 480 °FExtrusion
Mold Temperature 60.0 - 90.0 °FInjection
Injection Pressure 200 - 800 psiInjection
Back Pressure 25.0 - 100 psiInjection
Cushion 0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpmExtrusion
 50 - 100 rpmInjection
 
Descriptive Properties
AppearanceClear/Transparent

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ0869 / 237360

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.