LNP LUBRICOMP NL001 compound is based on Polycarbonate / Acrylonitrile Butadiene Styrene (PC/ABS) blend containing 5% PTFE. Added features of this grade include: Wear Resistant, suitable for Thin Wall applications. Features: Thin Wall,Wear resistant Information provided by SABIC |