MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Ascend Performance Materials HiDura™ D1MG33H BK0814 PA612-GF33
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612); Nylon 612, Glass Fiber Filler

Material Notes: HiDura™ D1MG33H BK0814 is a heat stabilized, 33% glass filled PA612 material designed for injection molding applications.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.32 g/ccDAM; ISO 1183
Moisture Absorption at Equilibrium 0.84 %DAM to 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0050 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.012 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 125 MPa50% RH; ISO 527-2
 163 MPaDAM; ISO 527-2
Elongation at Break 3.7 %DAM; ISO 527-2
 5.8 %50% RH; ISO 527-2
Tensile Modulus 7900 MPa50% RH; ISO 527-2
 9600 MPaDAM; ISO 527-2
Flexural Strength 183 MPa50% RH; ISO 178
 235 MPaDAM; ISO 178
Flexural Modulus 7600 MPa50% RH; ISO 178
 9100 MPaDAM; ISO 178
Izod Impact, Notched (ISO) 9.60 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 180/1A
 10.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 180/1A
 11.0 kJ/m²
@Temperature -40.0 °C
DAM; ISO 180/1A
 11.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
 13.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
 13.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
Charpy Impact Unnotched 71.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eU
 72.0 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 179/1eU
 79.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eU
 80.0 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eU
 82.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
 89.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
Charpy Impact, Notched 10.0 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 179/1eA
 10.0 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eA
 10.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
 11.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 13.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
 14.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 35.0 kV/mm
@Thickness 1.00 mm
DAM; IEC 60243
 36.0 kV/mm
@Thickness 1.00 mm
50% RH; IEC 60243
 
Thermal PropertiesOriginal ValueComments
Melting Point 218 °CDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 206 °CUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 190 °CUnannealed; 50% RH; ISO 75-2/A
 192 °CUnannealed; DAM; ISO 75-2/A
 
Processing PropertiesOriginal ValueComments
Melt Temperature 235 - 290 °CInjection
Mold Temperature 50.0 - 90.0 °CInjection
Drying Temperature 80.0 °CInjection
Dry Time 4.00 - 6.00 hourInjection
Moisture Content 0.15 %Injection
 
Descriptive Properties
AdditiveHeat Stabilizer
AppearanceBlack
Automotive Material SpecificationGM GMW17599P-PA612-GF35
FeaturesChemical Resistant
 Hydrolysis Resistant
 Medium-High Viscosity
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe, Asia Pacific

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASCE9004 / 287545

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.