MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BASF 2-Ethylhexyl Choroformate
Categories: Fluid

Material Notes: Formula: C9H17ClO2

CAS: 24468-16-1

Description: 2-Ethylhexyl Chloroformate is a colorless to yellowish liquid with a pungent odor. It hydrolyzes in the presence of water.

Synonyms: Chloroformic acid 2-ethylhexyl ester, Carbonochloridic acid, 2ethylhexyl ester

Applications: Intermediate used in Plastics processing and Organic peroxide.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.988 g/cc
Molecular Weight 192.7 g/mol
 
Thermal PropertiesOriginal ValueComments
Melting Point <= -55.0 °C
Flash Point 87.0 °C
Ignition Temperature 215 °C
 
Descriptive Properties
Assay>99%
Color<25APHA, DIN EN 1557
Composition2-Ethylhexanol<0.25%
 Alkyl chloride<0.03%
 Bis(2ethylhexyl)carbonate<0.5%
 Fe<5 ppm
 HCl<0.05%
 Phosgene<0.01%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF 5-Chlorovalerylchloride
BASF Basotect UF Foam
BASF Basotect TG Foam
BASF Basotect G Foam
BASF 4-Ethyl-1-octyn-3-ol

PBASG0955 / 132588

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.