LNP LUBRICOMP C2801 compound is based on Polycarbonate / Acrylonitrile Butadiene Styrene (PC/ABS) blend containing 5% PTFE. Added features of this grade include: Wear Resistant and Flame Retardant suitable for moving components in business equipment. Medium Heat performance. Features: Flame Retardant,Wear resistant Information provided by SABIC |