MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Osterman & Co Osterlene® LLM1018 LLDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Product Description: LLM1018 is best suited for applications requiring excellent clarity, gloss, toughness and heat seal. Typical blown film applications include; seal layer in coextrusions, heavy duty packaging and clarity packaging.

Availability: North America
Additive: Antiblock: No; Slip: No; Processing Aid: Yes
Features: Good Toughness; High Clarity; High Gloss
Uses: Packaging
Processing Method: Coextrusion

Information provided by Osterman & Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.918 g/cc0.0332 lb/in³ASTM D1505
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Puncture Resistance 77.0 N17.3 lb (f)ASTM D3763
Film Tensile Strength at Yield, MD 12.8 MPa1850 psiASTM D882
Film Tensile Strength at Yield, TD 10.0 MPa1450 psiASTM D882
Film Elongation at Break, MD 500 %500 %ASTM D882
Film Elongation at Break, TD 600 %600 %ASTM D882
Secant Modulus, MD 0.179 GPa26.0 ksiASTM D790
Secant Modulus, TD 0.208 GPa30.2 ksiASTM D790
Puncture Energy 6.28 J4.63 ft-lbASTM D3763
Film Tensile Strength at Break, MD 74.5 MPa10800 psiASTM D882
Film Tensile Strength at Break, TD 56.5 MPa8200 psiASTM D882
 
Descriptive Properties
Sealing Initial Temperature216°FASTM F88

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

POSTER121 / 267703

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.