MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger TECAPEI™ shapes combine Ultem® PEI polymer with Ensinger's proprietary extrusion techniques for exceptional reliability, consistency, dimensional stability, and high temperature mechanical performance. FDA, USP Class VI and NSF compliant.

SABIC ULTEM™ Resin 2300 Polyetherimide (PEI) (Americas)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification, KTW certification in recognized colors.

Features: High Stiffness,Hydrolytic Stability,Chemical Resistance,Low Smoke and Toxicity,Good Mechanicals in Broad Temperature Range,Low Creep Sensitivity,Good metal adhesion,Amorphous,High Strength,General Purpose,High Heat Resistance,Good dimensional stability,Flame Retardant

Information provided by SABIC

Vendors: Drake extrudes shapes and machines and injection molds parts in Torlon® PAI, PEEK, PAEK, Ryton PPS and Ultem PEI. It also machines Vespel® PI. Innovations include cryogenic CryoDyn® CT-200 shapes as a PCTFE alternative; efficient Seamless Tube® and the largest extruded rod diameters to >254mm and plate thicknesses to > 100mm. Certified to ISO 9001:2015 and AS9100D. Visit www.DrakePlastics.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.51 g/cc1.51 g/ccASTM D792
Water Absorption 0.16 %
@Time 86400 sec
0.16 %
@Time 24.0 hour
ASTM D570
Moisture Absorption 0.0200 %0.0200 %Injection Molding
Water Absorption at Saturation 0.90 %0.90 %ASTM D570
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm
@Thickness 3.20 mm
0.0020 - 0.0040 in/in
@Thickness 0.126 in
SABIC method
Linear Mold Shrinkage, Transverse 0.0020 - 0.0040 cm/cm
@Thickness 3.20 mm
0.0020 - 0.0040 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 5.0 g/10 min
@Load 6.60 kg,
Temperature 337 °C
5.0 g/10 min
@Load 14.6 lb,
Temperature 639 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 114114ASTM D785
Tensile Strength at Break 158 MPa22900 psi5 mm/min; ASTM D638
Tensile Strength, Yield 168 MPa24400 psi5 mm/min; ASTM D638
Elongation at Break 3.0 %3.0 %5 mm/min; ASTM D638
Tensile Modulus 9.30 GPa1350 ksi5 mm/min; ASTM D638
Flexural Strength 227 MPa32900 psibrk, 2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 8.96 GPa1300 ksi2.6 mm/min, 100 mm span; ASTM D790
Izod Impact Notched 85.0 J62.7 ft-lbASTM D256
 491 J
@Thickness 3.20 mm
362 ft-lb
@Thickness 0.126 in
reverse notched; ASTM D256
Izod Impact, Unnotched 4.27 J/cm8.00 ft-lb/inASTM D4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.00e+16 ohm-cm3.00e+16 ohm-cmASTM D257
Dielectric Constant 3.7
@Frequency 1000 Hz
3.7
@Frequency 1000 Hz
ASTM D150
Dielectric Strength  24.8 kV/mm
@Thickness 1.60 mm
630 kV/in
@Thickness 0.0630 in
in air; ASTM D149
 30.3 kV/mm
@Thickness 1.60 mm
770 kV/in
@Thickness 0.0630 in
in oil; ASTM D149
Dissipation Factor  0.0015
@Frequency 1000 Hz
0.0015
@Frequency 1000 Hz
ASTM D150
 0.0053
@Frequency 2.45e+9 Hz
0.0053
@Frequency 2.45e+9 Hz
ASTM D150
Arc Resistance 60 - 120 sec60 - 120 secASTM D495
Comparative Tracking Index 100 - 175 V100 - 175 VUL 746A
Hot Wire Ignition, HWI  15 - 30 sec
@Thickness >=1.50 mm
15 - 30 sec
@Thickness >=0.0591 in
UL 746A
 60 - 120 sec
@Thickness >=3.00 mm
60 - 120 sec
@Thickness >=0.118 in
UL 746A
High Amp Arc Ignition, HAI  0.00 - 15 arcs
@Thickness >=3.00 mm
0.00 - 15 arcs
@Thickness >=0.118 in
UL 746A
 15 - 30 arcs
@Thickness >=1.50 mm
15 - 30 arcs
@Thickness >=0.0591 in
UL 746A
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min3.15 - 5.91 in/minUL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  18.0 µm/m-°C
@Temperature -20.0 - 150 °C
10.0 µin/in-°F
@Temperature -4.00 - 302 °F
ISO 11359-2
 19.8 µm/m-°C
@Temperature -20.0 - 150 °C
11.0 µin/in-°F
@Temperature -4.00 - 302 °F
ASTM E831
CTE, linear, Transverse to Flow 48.0 µm/m-°C
@Temperature -20.0 - 150 °C
26.7 µin/in-°F
@Temperature -4.00 - 302 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 212 °C
@Thickness 6.40 mm
414 °F
@Thickness 0.252 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
@Thickness 6.40 mm
410 °F
@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point 227 °C441 °FRate B/50; ASTM D1525
UL RTI, Electrical 180 °C356 °FUL 746B
UL RTI, Mechanical with Impact 170 °C338 °FUL 746B
UL RTI, Mechanical without Impact 180 °C356 °FUL 746B
Flammability, UL94  V-0
@Thickness >=0.250 mm
V-0
@Thickness >=0.00984 in
UL 94
 5VA
@Thickness >=1.20 mm
5VA
@Thickness >=0.0472 in
UL 94
Smoke Density 1.61.6Flaming, Ds 4 min; ASTM E662
Oxygen Index 50 %50 %ASTM D2863
Glow Wire Ignition Temperature 900 °C
@Thickness 2.00 mm
1650 °F
@Thickness 0.0787 in
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 345 - 400 °C653 - 752 °F
Zone 2 340 - 400 °C644 - 752 °F
Zone 3 345 - 400 °C653 - 752 °F
Melt Temperature 350 - 400 °C662 - 752 °FInjection Molding
Mold Temperature 135 - 165 °C275 - 329 °F
Drying Temperature 150 °C302 °FInjection Molding
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hourInjection Molding
 24.0 hour24.0 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 40 - 60 %40 - 60 %
Vent Depth 0.00250 - 0.00760 cm0.000984 - 0.00299 in
Screw Speed 40 - 70 rpm40 - 70 rpm
 
Descriptive Properties
UV-light, water exposure/immersionF1UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82526 / 290473

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.