MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Lubrizol Advanced Materials PEARLBOND® 121 Linear Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Pearlbond™ 121 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines an extremely high crystallization rate with a very high thermoplasticity level. It is used for Hot Melt adhesives.

Application: Pearlbond™ 121 is mainly used for textile coating for making shoe-stiffeners (toe puffs & counters), by extrusion or sintering process. Pearlbond™ 121 can be used for making heat-sealable fabrics (thermobonding), obtained by coating processes such as scattering or dot-coating (powder or paste). In all cases, the product is previously ground into powder, by cryogenic grinding. The particle size of the powder will depend on the application technique to be used.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³ISO 2781
Viscosity 380000 cP
@Temperature 160 °C
380000 cP
@Temperature 320 °F
Melt viscosity @ 2.16 kg; ISO 1133
Melt Flow 30 - 60 g/10 min
@Load 2.16 kg,
Temperature 170 °C
30 - 60 g/10 min
@Load 4.76 lb,
Temperature 338 °F
PMES11
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5454ISO 868
 
Thermal PropertiesMetricEnglishComments
Melting Point 63.0 - 67.0 °C145 - 153 °FMQSA 70 A
Softening Point 55.0 - 60.0 °C131 - 140 °FMQSA 70 A
 
Descriptive Properties
Crystallization rate (minutes)Very highMQSA 12 B
ThermoplasticityVery highMQSA 68 A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lanxess Uniplex 512 Plastic Additive
ExxonMobil Escorene™ UL 05540EH2 Ethylene Vinyl Acetate Copolymer (European Grade)

PMES11 / 52909

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.