MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC LEXAN™ Copolymer XHT2143 PC (Asia)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: XHT2143 is a high flow, UV stabilized, high heat polycarbonate copolymer with an HDT/Af of 142 C. It is available in a range of opaque and limited transparent colors.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Density 1.20 g/ccISO 1183
Moisture Absorption 0.230 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.30 %ISO 62
Linear Mold Shrinkage, Flow 0.0060 - 0.0090 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 43 g/10 min
@Load 2.16 kg,
Temperature 330 °C
MVR, cm^3/10 min; ISO 1133
 46 g/10 min
@Load 2.16 kg,
Temperature 330 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 60.0 MPa50 mm/min; ISO 527
 60.0 MPaType I, 50. mm/min; ASTM D638
Tensile Strength, Yield 70.0 MPa50 mm/min; ISO 527
 70.0 MPaType I, 50 mm/min; ASTM D638
Elongation at Break 90 %50 mm/min; ISO 527
 90 %Type I, 50 mm/min; ASTM D638
Elongation at Yield 6.5 %50 mm/min; ISO 527
 6.5 %Type I, 50 mm/min; ASTM D638
Flexural Yield Strength 100 MPa2 mm/min; ISO 178
 110 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2450 MPa2 mm/min; ISO 178
 2550 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 115 J/mASTM D256
 75.0 J/m
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 11.0 kJ/m²80*10*4; ISO 180/1A
 10.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 20.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Instrumented Impact Total Energy 68.0 JASTM D3763
Tangent Modulus 2600 MPa1 mm/min; ISO 527
 2600 MPa5 mm/min; ASTM D638
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E 831
 60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E 831
 60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 155 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 142 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 145 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 160 °CRate B/50; ISO 306
 161 °CRate B/50; ASTM D1525
 162 °CRate B/120; ISO 306
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 285 - 325 °C
Zone 1 270 - 310 °C
Zone 2 280 - 320 °C
Zone 3 290 - 330 °C
Melt Temperature 290 - 330 °C
Mold Temperature 85.0 - 130 °C
Drying Temperature 135 °C
Dry Time 4.00 - 6.00 hour
Moisture Content 0.020 %
Back Pressure 0.300 - 0.700 MPa
Shot Size 40 - 60 %
Vent Depth 0.00250 - 0.00800 cm
Screw Speed 40 - 90 rpm

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lotte Advanced Materials Infino® SC-1220UR PC, Unreinforced

PSABI21821 / 214957

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.