MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Akrochem AKROSPERSE® Sb2O3-85/EPR/S Dispersion
Categories: Other Engineering Material

Material Notes: Product Description: Akrosperse Sb2O3 is a dispersion of 85% active antimony oxide in an EPR (ethylene-propylene copolymer) binder. Antimony trioxide (commonly called antimony oxide) is used as a synergistic fire retardant in elastomeric systems. By itself, Sb2O3 offers no flame resistance; it must be used in conjunction with a halogen (Cl or Br typically) source to effect the burning process. HCl formed from the chlorine source reacts with Sb2O3 to form antimony trichloride which then reacts with hydroxyl radicals in the pyrolysis zone to short-circuit the propagation of the combustion reaction.

Applications: Akrosperse Sb2O3 is an excellent flame retarder for elastomeric and plastic compounds with a typical loading range of 4 - 20phr. Chlorine-bearing additives like chlorinated paraffins (Akrochlor?) should be added at a 10-30 phr level (Note: EPDM is not highly compatible with chlorinated paraffins. Use a higher molecular weight chlorinated resin to prevent bleed). Halogenated compounds (CR, NBR/PVC) may not require additional halogen donors. The rubber-bound form is a proven method of reducing skin irritation sometimes produced by handling antimony trioxide. The use of Sb2O3 and Cl to reduce fire has the drawback of creating more smoke in a fire (sometimes acidic smoke due to the HCl present). A compounder should use alumina trihydrate (ATH) along with the Sb2O3 system to reduce smoke as much as possible in rubber compounds. In plastic compounds, the use of magnesium hydroxide (Versamag®) or magnesium carbonate (Elastocarb®) will decrease smoke levels.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 3.10 g/cc
 
Descriptive Properties
AppearanceOff-white rubber slabs
Content0.85Sb2O3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH248 / 315166

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.