LNP THERMOCOMP DC006ERH compound is based on Polycarbonate (PC) resin containing 30% carbon fiber. Added features of this grade include: Electrically Conductive, Easy Molding, Mold Release, Healthcare. Features: Healthcare,High Stiffness,Light-weight Structural,Super Strong (Carbon Fiber Filled),Good Mold Release,Electrically Conductive,Easy Molding,Structural Information provided by SABIC |