MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Nouryon Butanox M-50 RED YM 1:6 Methyl ethyl ketone peroxide in dimethyl phthalate
Categories: Other Engineering Material

Material Notes: General purpose MEKP for the curing of unsaturated polyester resins in the presence of a cobalt accelerator at room and elevated temperatures, including a red indicator system.

CAS number: 1338-23-4

EINECS/ELINCS No.: 215-661-2

Applications: Butanox M-50 RED YM 1:6 is a general purpose methyl ethyl ketone peroxide (MEKP) for the curing of unsaturated polyester resins in the presence of a cobalt accelerator at room and elevated temperatures. Butanox M-50 RED YM 1:6 offers all the advantages of a standard MEKP i.e. Butanox M-50. The Butanox M-50 RED YM 1:6 includes a red indicator system that in most cases almost disappears during cure. The red color is there when you need it i.e. during the mixing step, but will fade away during cure. The curing system Butanox M-50 RED YM 1:6/cobalt accelerator is particularly suitable for the curing of gelcoat resins, laminating resins, lacquers and castings; moreover the manufacture of light resistant parts may be possible contrary to the curing system benzoyl peroxide/amine accelerator. Practical experience throughout many years has proven that by the guaranteed low water content and the absence of polar compounds in Butanox M-50 RED YM 1:6, this peroxide is very suitable in GRP products for e.g. marine applications. For room temperature application it is necessary to use Butanox M-50 RED YM 1:6 together with a cobalt accelerator (e.g. Accelerator NL-49P).

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³
Viscosity 24 cP24 cP
Storage Temperature <= 25.0 °C<= 77.0 °F
 
Thermal PropertiesMetricEnglishComments
Decomposition Temperature 70.0 °C158 °FSelf-Accelerating Decomposition Temperature
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 3.0 %<= 3.0 %
 
Descriptive Properties
AppearanceRed liquid
Content8.8-9.0 %Total active oxygen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY447 / 285970

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.