MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Arkema Pebax® MX 1205 Polyether Block Amide (PEBA)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyether Block Amide (PEBA)

Material Notes: Typical application: Impact modifier

Information provided by Arkema Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³ASTM D792
Water Absorption 1.2 %1.2 %24 hr in water at 20°C; ASTM D570
Moisture Absorption at Equilibrium 0.40 %0.40 %20°C and 65% RH; ASTM D570
Melt Flow 9.0 g/10 min9.0 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4242ASTM D2240
Tensile Strength at Break 36.0 MPa5220 psiASTM D638
Elongation at Break 600 %600 %ASTM D638
Flexural Modulus 0.0780 GPa11.3 ksiASTM D790
Izod Impact, Notched NBNBASTM D256-A
 NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
ASTM D256-A
Izod Impact, Unnotched NBNBASTM D256-A
 NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
ASTM D256-A
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 3.00e+12 ohm
@Temperature 20.0 °C
3.00e+12 ohm
@Temperature 68.0 °F
65% RH; ASTM D257
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 22.0 J/g9.46 BTU/lbASTM D3417
CTE, linear 200 µm/m-°C
@Temperature -40.0 - 140 °C
111 µin/in-°F
@Temperature -40.0 - 284 °F
ASTM D696
Melting Point 147 °C297 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 52.0 °C126 °FASTM D648
Vicat Softening Point 114 °C237 °Funder 1 daN; ASTM D1525

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema Pebax® Rnew® 55R53 SP 01 Polyether Block Amide (PEBA)
Arkema Pebax® MV 3000 SP 01 Polyether Block Amide (PEBA)
Arkema Pebax® MV 2080 Polyether Block Amide (PEBA)
Arkema Pebax® MV 1074 SP 01 Polyether Block Amide (PEBA)
Arkema Pebax® MV 1074 SA 01 MED Polyether Block Amide (PEBA)

PZARKG537 / 24410

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.