MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Kolon KOPEL® KP3942BM Thermoplastic Polyester Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE

Material Notes: Blow molding, TPC-ET

Flexibility and elastic recovery are similar to rubber, but the mechanical properties, heat resistance, weather resistance and UV stability are far better than the performance of conventional rubber.

Information provided by Kolon Plastic, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 g/cc1.15 g/ccISO 1183
Water Absorption 0.40 %
@Time 86400 sec
0.40 %
@Time 24.0 hour
ISO 62
Linear Mold Shrinkage 0.015 - 0.019 cm/cm0.015 - 0.019 in/inISO 294-4
Melt Flow 4.0 g/10 min
@Load 5.00 kg,
Temperature 230 °C
4.0 g/10 min
@Load 11.0 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D <= 42<= 42ISO 868
Tensile Strength at Break 21.0 MPa
@Thickness 2.00 mm
3050 psi
@Thickness 0.0787 in
50 mm/min; ISO 527
Elongation at Break 450 %
@Thickness 2.00 mm
450 %
@Thickness 0.0787 in
50 mm/min; ISO 527
Flexural Modulus 0.104 GPa
@Thickness 4.00 mm
15.1 ksi
@Thickness 0.157 in
10 mm/min; ISO 178
 
Thermal PropertiesMetricEnglishComments
Melting Point 200 °C392 °F20 ?/min; ISO 11357-1
Vicat Softening Point 154 °C
@Load 1.02 kg
309 °F
@Load 2.25 lb
50°C/h; ISO 306
Flammability, UL94 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 190 - 210 °C374 - 410 °F
Middle Barrel Temperature 210 - 230 °C410 - 446 °F
Front Barrel Temperature 220 - 240 °C428 - 464 °F
Nozzle Temperature 220 - 240 °C428 - 464 °F
Mold Temperature 20.0 - 40.0 °C68.0 - 104 °F
Drying Temperature 80.0 - 110 °C
@Time 10800 - 21600 sec
176 - 230 °F
@Time 3.00 - 6.00 hour
Dehumidifying Dryer
Moisture Content <= 0.080 %<= 0.080 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKOKZ783 / 255794

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.