MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Go Yen Chemical GGK-T-1022 Environmental Catalyst
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: GGK-T-1022 is mainly used as catalyst in ester exchange & condensation reaction of organic synthetic, adhesive for metal, plastic, rubber, plastic modifier, paint additive, all kinds of expandable polystyrene, polyester, nylon, environmental catalyst in PU polymerization processing, medical organic synthetic, modifiers, cross-linking agents, synthetic dispersing agents, and various kinds of fine chemicals.

Characteristic:

  • Odorless
  • Lower toxic
  • Easy to burning
  • Deliquesce while meeting water or humid air
  • Easy to be resin material while heated

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.960 - 1.00 g/cc0.0347 - 0.0361 lb/in³
pH 6.06.0
 
Thermal PropertiesMetricEnglishComments
Boiling Point 154 °C
@Pressure 0.0133 MPa
309 °F
@Pressure 1.93 psi
Flash Point 60.0 °C140 °FOpen cup
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4625 - 1.46451.4625 - 1.4645
 
Descriptive Properties
Appearancetransparent to light yellow proper liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOYEN540 / 266848

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.