MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Diofan® A 602 PVDC
Categories: Polymer; Thermoplastic; Polyvinyl Dichloride (PVDC); Polyvinyl Dichloride (PVDC)

Material Notes: Diofan® A 602 is a water based dispersion of a polyvinylidene chloride copolymer. It is free of solvent traces, alkylphenol ethoxylates or any other toxic substances.

It features strong barrier properties to water vapor and very low water absorption. Diofan® A 602 also offers very good resistance to oil and benzene. Due to a very low MFFT, this waterborne binder can be applied at low temperature as a flexible and tack free film.

Diofan® A 602, as chlorinated based latex, combines also fire retardant properties. End uses are for example:
- Barrier and sealing coatings
- Flame resistant coatings
- Fiber and textile coatings

Substrates can be concrete, cement, wood, gypsum, paper, fiberboard, fabrics and others.

Applications: Barrier Coatings; Coating Applications

Features: Flame Retardant; Low to No Water Absorption; Moisture Barrier; Non-Toxic; Oil Resistant; Oxygen BarrierDiofan® A 602 is delivered in bulk or in Intermediate Bulk Containers (IBC). Bulk supplied latex should be stored in reservoirs made of suitable stainless steel, HDPE, rigid PVC or glass fiber-reinforced polyester.
- Contact of anionic Diofan® dispersion with metals like iron, zinc, aluminum and copper as well as alloys such as brass and bronze must be avoided.
- Keep the vessels tightly closed to prevent drying through evaporation. Store the product ideally between 5°C and 30°C (41 °F and 86°F) to avoid degradation.

PROCESSING - DRYING
- Diofan® A 602 can be processed with different coating techniques, including reverse gravure roll and air knife coating systems.
- When coated on plastic films, Diofan® A 602 should be formulated with wax and silica in order to improve the blocking and slip properties of the finished coating.
- Diofan® coatings requires adequate drying conditions, since in general higher temperatures will contribute to better barrier properties.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.26 g/cc
pH 4.0
Water Vapor Transmission 160 g/m²/day
@Thickness 0.00100 mm,
Temperature 38.0 °C
90% RH; ASTM F1249
Viscosity 19 cP
@Temperature 23.0 °C
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 7.00 °CDSC
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorMilky White
FormsLiquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4169 / 279969

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.