MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Carbon Printers FPU 50 Flexible Polyurethane
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polyurethane, TP

Material Notes: FPU 50 is an impact, abrasion and fatigue resistant semi-rigid material that is a good choice for parts that must withstand repetitive stresses such as living hinges or friction fits.

Information provided by Carbon®

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.053 g/ccASTM D792
 1.06 g/ccliquid resin
Water Absorption 0.75 %long term; ASTM D570
 0.42 %
@Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 71ASTM D2240
Tensile Strength, Ultimate 28.0 - 30.0 MPaType V, 10 mm/min; ASTM D638
Tensile Strength, Yield 19.0 - 21.0 MPaType V, 10 mm/min; ASTM D638
Elongation at Break 265 - 295 %Type V, 10 mm/min; ASTM D638
Elongation at Yield 6.0 - 8.0 %Type V, 10 mm/min; ASTM D638
Tensile Modulus 750 - 970 MPaType V, 10 mm/min; ASTM D638
Flexural Strength 31.0 - 33.0 MPa
@Strain 5.0 %
no yielding; ASTM D790-B
Flexural Modulus 795 - 867 MPa
@Strain 0.5 - 1 %
Chord; ASTM D790-B
Izod Impact, Notched 24.0 - 36.0 J/m
@Temperature -30.0 °C
Machined; ASTM D256
 35.0 - 45.0 J/m
@Temperature 23.0 °C
Machined; ASTM D256
Izod Impact, Unnotched NBASTM D4812
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.87e+13 ohm-cmASTM D257
Dielectric Constant 3.21
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 13.0 kV/mmASTM D149
Dissipation Factor 0.0131
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 129 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Specific Heat Capacity 1.48 J/g-°CASTM E1269
Thermal Conductivity 0.138 W/m-KASTM C518
Deflection Temperature at 0.46 MPa (66 psi) 78.0 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 52.0 °CASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCARBP016 / 255848

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.