MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Marco Polo MARPOL EVA 1707 EVA
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Film Grade

Material Notes: MARPOL® EVA 1707 is a 17.2 wt% vinyl acetate copolymer film resin with excellent strength and toughness. It also displays excellent optics and sealing properties.

Recommended Applications: Heat seal layer, pallet shrink film, stretch film.

Additives: Antiblock – no, Slip – no.

Information provided by Marco Polo International, LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.939 g/ccASTM D1505
Vinyl Acetate Content 17.2 %
Melt Flow 0.70 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 370 %ASTM D882
Film Elongation at Break, TD 660 %ASTM D882
Flexural Modulus, 1% Secant 9200 psiMD; ASTM D882
 10000 psiTD; ASTM D882
Elmendorf Tear Strength MD 50 gASTM D1922
Elmendorf Tear Strength, MD 120 g/milASTM D1922
Dart Drop Test 650 gASTM D1709A
Film Tensile Strength at Break, MD 5300 psiASTM D882
Film Tensile Strength at Break, TD 5300 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 87.0 °CPeak; ASTM D3418
Vicat Softening Point 66.0 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 1.3 %ASTM D1003
Gloss 87 %45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMARCO210 / 283807

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.