MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

Caplinq LINQTAPE™ PIT1N-Alum 1-mil Polyimide Film with Sputtered Aluminized Coating
Categories: Polymer; Adhesive; Thermoset; Polyimide, TS; Polyimide, Thermoset Film

Material Notes: CAPLINQ Linqstat™ PIT1N-Alum Series is a high performance, high-temperature resistant aluminized polyimide film, formed by sputtering aluminum on to polyimide using an aluminum vacuumed position method. This combination of materials allows that one side is an insulation side and the other is conductive. CAPLINQ Linqstat™ PIT1N-Alum Series combines these two materials to give a very heat resistant, mechanically and chemically stable, radiation-resistant, and self-extinguishing product that has very high thermal conductivity and EMI shielding. CAPLINQ Linqstat™ PIT1N-Alum Series is a used in a number of applications, including as a first surface mirror for multi layer insulation (MLI) blankets, EMI shielding, electromagnetic shielding tape and flexible etching wire.

Applications:

  • Best absorption/ emittance/ cost combination
  • Cost effective radiative transfer barrier
  • Excellent high temperature stability
  • Excellent burn resistance
  • Multilayer Insulation (MLI) blankets
  • EMI shielding
  • Flexible Etching Wire
  • First or second surface mirror

Information provided by Caplinq

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 0.102 microns0.00400 milAluminum Coating
 25.4 microns1.00 milFilm (Backing)
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD >= 75 %>= 75 %
Film Elongation at Break, TD >= 75 %>= 75 %
Film Tensile Strength at Break, MD >= 200 MPa>= 29000 psi
Film Tensile Strength at Break, TD >= 175 MPa>= 25400 psi
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square <= 1.0 ohm<= 1.0 ohmAluminum
 >= 3.0 ohm>= 3.0 ohm
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Inert 400 °C752 °FIntermittent
 400 °C752 °FContinuous
Minimum Service Temperature, Air -250 °C-418 °FIntermittent
 -250 °C-418 °FContinuous
Flammability, UL94 V-0V-0
 
Descriptive Properties
Adhesion TypeNone
ColorAmber/Gold
First surface<0.035 eHsolar emittance
 <0.14 asolar absorptance

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCAPL1010 / 256010

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.