MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC NORYL WCD841U PPE-TPE  (Unverified Data**)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyphenylene Ether/PPO

Material Notes: Flexible, UV stabilized, halogen free extrusion grade for applications such as wire insulation and cable jacket. Good color stability after UV weathering per ASTM D4459. Light color capable. Flame retardant performance capable of meeting UL VW-1 requirement. 80C application temperature rating as defined by UL 1581. 84 Shore A hardness. Processing typically conducted on standard extrusion equipment. UL 1581 tests conducted on 2.0 mm wire with 0.12 mm x 20 stranded copper conductor.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.08 g/ccASTM D792
Melt Flow 23 g/10 min
@Load 5.00 kg,
Temperature 250 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 8430S reading; ASTM D2240
Tensile Strength at Break 17.0 MPa50 mm/min; ISO 527
 18.0 MPaUL 1581
 18.0 MPaType I, 50 mm/min; ASTM D638
 20.0 MPaafter 7days @113°C; UL 1581
Elongation at Break 220 %50 mm/min; ISO 527
 238 %after 7days @113°C; UL 1581
 250 %Type I, 50 mm/min; ASTM D638
 295 %UL 1581
Flexural Modulus 90.0 MPa12.5 mm/min, 100 mm span; ASTM D790
 90.0 MPa12.5 mm/min; ISO 178
Heat Distortion 19 %
@Load 0.250 kg,
Temperature 100 °C
UL 1581
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 4.20e+15 ohm-cmASTM D257
Dielectric Constant 2.6
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 21.5 kV/mm
@Thickness 2.00 mm
in oil; IEC 60243-1
Dissipation Factor 0.0060
@Frequency 1e+6 Hz
ASTM D150
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 80.0 °CUL temperature rating; UL 1581
Brittleness Temperature <= -40.0 °CASTM D746
Smoke Density <= 133
@Thickness 0.500 mm
0.5 mm plaque, Flame, Ds, max; ASTM E 662
 <= 170
@Thickness 0.500 mm
0.5 mm plaque, Non-flame, Ds, max; ASTM E 662
Oxygen Index 25 %ISO 4589
Glow Wire Ignition Temperature 750 °CIEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Descriptive Properties
VW-1PassUL 1581

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI52698 / 152744

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.