MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC NORYL™ Resin NH5110E Polyphenylene Ether + PS (PPE+PS)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ NH5110E resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This extrusion grade contains non-brominated, non-chlorinated flame retardant and carries a UL94 flame rating of V1 at 1.5mm along with a Vicat B/120 temperature of 138C according to ISO 306. NORYL NH5110E resin was developed for low-beard growth during profile extrusion and is an excellent candidate for electrical conduit and cable management applications.

Features: Low Creep Sensitivity,Non-Halogenated,Non-Chlorinated,Non-Brominated

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.09 g/ccISO 1183
Moisture Absorption 0.0600 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.15 %ISO 62-1
Viscosity 9.0 cP
@Load 5.00 kg,
Temperature 280 °C
MVR cc/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 52.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 64.0 MPa50 mm/min; ISO 527
Elongation at Break 18 %50 mm/min; ISO 527
Elongation at Yield 4.0 %50 mm/min; ISO 527
Tensile Modulus 2500 MPa1 mm/min; ISO 527
Flexural Strength 98.0 MPayield, 2 mm/min; ISO 178
Flexural Modulus 2400 MPa2 mm/min; ISO 178
Izod Impact, Notched (ISO) 24.0 kJ/m²80*10*4; ISO 180/1A
 9.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 26.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 11.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.6
@Frequency 1e+6 Hz
ASTM D150
 2.6
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 46.0 kV/mm
@Thickness 1.00 mm
shorttime; IEC 60243-1
Dissipation Factor 0.0017
@Frequency 1e+6 Hz
ASTM D150
 0.0017
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 82.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ASTM E831
 82.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 94.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ASTM E831
 94.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
Hot Ball Pressure Test 125 °CPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 129 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 114 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
Vicat Softening Point 138 °CRate B/120; ISO 306
 149 °CRate B/50; ISO 306
UL RTI, Electrical 65.0 °CUL 746B
UL RTI, Mechanical with Impact 65.0 °CUL 746B
UL RTI, Mechanical without Impact 65.0 °CUL 746B
Flammability, UL94 V-1
@Thickness 1.50 mm
UL 94
Oxygen Index 34 %ISO 4589
 
Processing PropertiesOriginal ValueComments
Processing Temperature 50.0 - 70.0 °CCalibrator Temperature
Zone 1 220 - 240 °CProfile Extrusion
Zone 2 230 - 250 °CProfile Extrusion
Zone 3 240 - 260 °CProfile Extrusion
Zone 4 240 - 260 °CProfile Extrusion
Adapter Temperature 240 - 260 °CProfile Extrusion
Die Temperature 240 - 260 °CProfile Extrusion
Melt Temperature 240 - 260 °CProfile Extrusion
Drying Temperature 80.0 - 90.0 °CProfile Extrusion
Dry Time 2.00 - 3.00 hourProfile Extrusion
Precipitation Temperature 40.0 - 60.0 °CHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82387 / 290334

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.