Intro: GO YEN CHEMICAL INDUSTRIAL CO., LTD. (GYC) Group always makes efforts to research and produce all types of water & oil repellent product. These high additional value series are already used to textile industries for many years. GOYENCHEM-920 belongs to solvent-based nano-fluorine structure. GOYENCHEM-920 do not use highly toxic solvent such as benzene, toluene or xylene for dilution. GOYENCHEM-920 can be widely used to various leather and textile materials processing. GOYENCHEM-920 provides good water & oil repellent? anti-stain and anti-dust performance, and still has good hand feeling?breathing ability and nature appearance after treated. Advantages: - Provide good water & oil repellent performance for textile and leather
- Provide anti-stain and anti-dust layer after treated
- Suitable for use on various textile and fabric products
- Can be used to several natural or synthetic leather
- Good hand feeling
- Excellent process stability
- Good penetrability and wetting property
- Excellent permeability
- Do not affect material features after treated
Using Method- Suitable for various textile and leather processing
- GOYENCHEM-920 can be sprayed and coated on leather and other surface
- Diluted liquid can be used by aerosol can
- Suggested dilution solvent : EAc?BAc?Hexane? Heptane?Butanone, the dilution can be adjusted 1 ~10 times by customer’s request.
- Spray and coating back and forth twice and evenly.
- Natural drying or heat drying (below 80?)
Information provided by Go Yen Chemical |