System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Dowhon DHF-60011F FFKM, Copolymer, Oring, Gasket
Categories:
Polymer
;
Thermoset
;
Fluoropolymer, TS
;
Thermoset Fluoroelastomer
Material Notes:
Property: good mold release, for various Oring and gaskets, low CS
Information provided by SICHUAN DOWHON NEW MATERIALS CO., LTD.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.91
g/cc
1.91
g/cc
Mechanical Properties
Metric
English
Comments
Hardness, Shore A
60
60
58
@Temperature 150 °C,
Time 252000 sec
58
@Temperature 302 °F,
Time 70.0 hour
OIL 903
61
@Temperature 250 °C,
Time 252000 sec
61
@Temperature 482 °F,
Time 70.0 hour
Aging
Tensile Strength
13.5
MPa
1960
psi
12.7575
MPa
@Temperature 250 °C,
Time 252000 sec
1850.32
psi
@Temperature 482 °F,
Time 70.0 hour
Aging
13.3515
MPa
@Temperature 150 °C,
Time 252000 sec
1936.47
psi
@Temperature 302 °F,
Time 70.0 hour
OIL 903
Elongation at Break
240 %
240 %
230.88 %
@Temperature 250 °C,
Time 252000 sec
230.88 %
@Temperature 482 °F,
Time 70.0 hour
Aging
249.36 %
@Temperature 150 °C,
Time 252000 sec
249.36 %
@Temperature 302 °F,
Time 70.0 hour
OIL 903
Compression Set
12 %
@Temperature 200 °C,
Time 252000 sec
12 %
@Temperature 392 °F,
Time 70.0 hour
ASTM D395 Method B
Thermal Properties
Metric
English
Comments
Minimum Service Temperature, Air
-18.0
°C
-0.400
°F
TR10
Brittleness Temperature
-26.0
°C
-14.8
°F
Descriptive Properties
Color
brown
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PDOWHON062 / 315974
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.