MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Angst+Pfister APSOplast® FEP Fluoro plastic
Categories: Polymer; Thermoplastic; Fluoropolymer; Fluorinated Ethylene Propylene (FEP)

Material Notes: General description: FEP is produced through the copolymerization of tetrafluoroethylene and hexafluoropropylene. Like PTFE, its carbon structure is completely surrounded by fluorine atoms. FEP is a thermoplastic which can be processed using traditional thermoplastic processing techniques such as screw extrusion, injection moulding, and blow extrusion. FEP can be thermoformed and is easy to weld.

Characteristics and properties:

  • Extremely broad service temperature range (long-term temperatures of –190 to +205 °C)
  • FEP is very tough and flexible even at low temperatures thanks to its high impact resistance
  • FEP has a low permeability with regard to gases and chemicals and is subject to practically no moisture absorption (less than 0.01%)
  • Excellent resistance to most chemicals and solvents except for liquid sodium, fluorine, chemicals at elevated temperatures, and certain halogen compounds
  • Good weather resistance
  • Good anti-adhesive properties
  • Excellent dielectric properties
  • The dielectric constant and loss factor of FEP are extremely low and relatively constant over a broad temperature and frequency range
  • High insulation resistance
  • High dielectric strength
  • Flame-retardant

Information provided by Angst + Pfister

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.15 g/ccDIN EN ISO 1183-1
Water Absorption at Saturation <= 0.050 %DIN EN ISO 62
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+17 ohm-cmDIN IEC 60023
Surface Resistance 1.00e+16 ohmDIN IEC 60023
Dielectric Constant 2.1
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 40.0 kV/mmIEC 60243-1
Dielectric Loss Index 0.00060
@Frequency 1e+6 Hz
after 24 h immersed in water; IEC 60250
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 85.0 - 105 µm/m-°C
@Temperature 23.0 - 95.0 °C
DIN 53752
Melting Point 285 °C
Minimum Service Temperature, Air -200 °C
 
Descriptive Properties
Colortransparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PANGP095 / 250593

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.