MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Celanese Hytrel® 4053FGF NC010 TPC-ET
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE

Material Notes: 40 Shore D High Performance Polyester Elastomer Developed for Food Contact Applications

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0020 cm/cm0.0020 in/inISO 294-4, 2577
Melt Flow 9.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
9.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 363615s; ISO 48-4
 <= 38<= 38ISO 48-4
Tensile Stress at Strain  2.50 MPa
@Strain 5.0 %
363 psi
@Strain 5.0 %
1BA specimen at 50mm/min; ISO 527-1/-2
 4.00 MPa
@Strain 10 %
580 psi
@Strain 10 %
ISO 527-1/-2
 7.00 MPa
@Strain 50 %
1020 psi
@Strain 50 %
ISO 527-1/-2
 8.00 MPa
@Strain 100 %
1160 psi
@Strain 100 %
ISO 527-1/-2
Tensile Modulus 0.0550 GPa7.98 ksiISO 527-1/-2
Flexural Modulus 0.0600 GPa8.70 ksiISO 178
Poissons Ratio 0.500.50
Charpy Impact, Notched  10.0 J/cm²
@Temperature -40.0 °C
47.6 ft-lb/in²
@Temperature -40.0 °F
ISO 179/1eA
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eA
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 148 °C298 °F10°C/min; ISO 11357-1/-3
Glass Transition Temp, Tg -50.0 °C-58.0 °F10°C/min; ISO 11357-1/-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 170 °C338 °FOptimum, Extrusion
 180 °C356 °FOptimum, Injection
Mold Temperature 35.0 °C95.0 °FOptimum, Injection
 30.0 - 40.0 °C86.0 - 104 °FInjection
Drying Temperature 80.0 °C176 °FInjection
 70.0 - 90.0 °C158 - 194 °FExtrusion
Dry Time 2.00 - 3.00 hour2.00 - 3.00 hourExtrusion, Dehumidified Dryer
 2.00 - 3.00 hour2.00 - 3.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.060 %<= 0.060 %Extrusion
 <= 0.080 %<= 0.080 %Injection
 
Descriptive Properties
Drying RecommendedyesInjection
Part Marking Code>TPC-ET<ISO 11469
PolymerTPC
Resin IdentificationTPC-ETISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDSX5173b / 254335

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.