MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Carbon Printers EPX 82 Epoxy, Dry
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoset; Epoxy

Material Notes: EPX 82 combines functional toughness, stiffness, and temperature resistance making it useful in a variety of automotive, industrial, and consumer applications.

Information provided by Carbon®

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.12 g/ccliquid resin
 1.155 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 89instant; ASTM D2240
 88
@Time 5.00 sec
ASTM D2240
Tensile Strength at Break 5.90 MPa
Tensile Strength, Ultimate 82.0 MPa
Elongation at Yield 5.5 %
Tensile Modulus 2800 MPa
Flexural Strength 130 MPa
@Strain 5.0 %
Flexural Modulus 3000 MPa
Izod Impact, Notched 44.0 J/mMachined; ASTM D256
Izod Impact, Unnotched 370 J/mASTM D4812
Charpy Impact Unnotched 26.0 kJ/m²ISO 179-1/1eU
Charpy Impact, Notched 4.40 kJ/m²Machined; ISO 179-1/1eA
Gardner Impact 0.550 J
@Thickness 3.20 mm
ASTM D5420 GC
Taber Abrasion, mg/1000 Cycles 42
@Load 1.00 kg
CS-17, 100 % vacuum; ASTM D4060
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 4.99e+15 ohm-cmASTM D257
Dielectric Constant 3.41
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 18.0 kV/mmASTM D149
Dissipation Factor 0.00714
@Frequency 1000 Hz
ASTM D150
Comparative Tracking Index 600 VASTM D3638
 
Thermal PropertiesOriginal ValueComments
CTE, linear 88.0 µm/m-°C
@Temperature -60.0 - 100 °C
ASTM E831
Specific Heat Capacity 1.33 J/g-°CASTM E1269
Thermal Conductivity 0.194 W/m-KASTM C518
Deflection Temperature at 0.46 MPa (66 psi) 130 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 120 °CASTM D648
Flammability, UL94 HB
@Thickness 1.50 mm
 HB
@Thickness 3.00 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCARBP005 / 255837

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.