Ultramid A3WC4 HP is a 20 wt. % short carbon fiber reinforced, heat stabilized, high flow PA66 injection molding grade. The Ultramid A3WC4 HP has excellent mechanical properties and is suitable for large injection molded components.Information provided by BASF. |