MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Konson Lithium Stearate for PVC Heat Stabilizer
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product name: Lithium Stearate

Molecular formula: C17H35COOLI

Application: Lithium Stearate can be used as PVC heat stabilizers in transparent products, when use in conjunction with phthalate plasticizers, the film transparency of products is good and does not appear white mist. Lithium Sterate is easier to melt in ketones compare with other stearates, thus little effect on the embossing operation. It is non-toxic substitute for barium soap and lead soap. The product can also be used in conjunction with the phospholipid acid plasticizers. This product can also be used as an external lubricant for nylon, phenolic resin, rigid polyvinyl chloride (maximum amount of 0.6 % ) In addition, the goods can be used as construction waterproof, impermeable and so on.

Information provided by Konson®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Particle Mesh Size 325 Mesh=99.5%
 
Thermal PropertiesOriginal ValueComments
Melting Point 220 - 221.5 °C
 
Descriptive Properties
Appearancewhite powder, with fat smell
Content<0.2%Free Acid
Loss of Drying=1.0%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKONS070 / 256115

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.